Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 490 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 254 °C
490 °F
Oxford Polymers PBT 30GF PBT, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and LubricantsSpecial Characteris..
Melt Temperature 254 - 266 °C
490 - 510 °F
ASTM D789
Niche Polymer PA66GF13N Nylon 66, 13% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 254 - 271 °C
490 - 520 °F
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy
Acrylonitrile Styrene Acrylate + PolycarbonatePreliminary DataProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In..
Melt Temperature 254 - 277 °C
490 - 530 °F
Ravago Manufacturing Americas Hylon® N2017THL Nylon 6 (DAM)
Information provided by Ravago.
Melt Temperature 254 - 277 °C
490 - 530 °F
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (DAM)
Information provided by Ravago.
Melt Temperature 254 - 271 °C
490 - 520 °F
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy
Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Melt Temperature 254 - 277 °C
490 - 530 °F
Ravago Manufacturing Americas Hylon® N2017STHL Nylon 6 (DAM)
Information provided by Ravago.
Melt Temperature 254 - 338 °C
490 - 640 °F
Average value: 296 °C Grade Count:7
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Melt Temperature 254 - 282 °C
490 - 540 °F
Molding
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)Information provided by PolyOne Corporation.
Melt Temperature 254 - 277 °C
490 - 530 °F
LTL Color Compounds ColorFast® FRPBT130 PBT, 30% Glass-Filled
30% glass-filled V-0 rated PBT - UL listedAll information provided by LTL Color Compounders, Inc.
Melt Temperature 254 - 277 °C
490 - 530 °F
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded
13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc.
Melt Temperature 254 - 271 °C
490 - 520 °F
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow
Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
Melt Temperature 254 - 282 °C
490 - 540 °F
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Melt Temperature 254 - 282 °C
490 - 540 °F
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Melt Temperature 254 - 282 °C
490 - 540 °F
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Melt Temperature 254 - 288 °C
490 - 550 °F
Ecomass® 1850ZD96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)RigidInformation provided by Technical Polymers
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced
Data provided by Clariant Masterbatches
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant 6004G8-HSL BK UV Black Nylon 6, 8% Glass Fiber Reinforced
Data provided by Clariant Masterbatches
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant 6008 L Nylon 6, High Impact, Injection Molding
Data provided by Clariant Masterbatches
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant PA213M40 Nylon 6, 40% Mineral Reinforced, Heat Stabilized
Data provided by Clariant Masterbatches
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black
Data provided by Clariant Masterbatches
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant Renol 6001 GP HSL Nylon 6, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant Renol 6253 Nylon 6, High Impact
Data provided by Clariant Masterbatches
Melt Temperature 254 - 282 °C
490 - 540 °F
Clariant Renol BR7140 Polycarbonate/ABS Alloy
Data provided by Clariant Masterbatches
Melt Temperature 254 - 282 °C
490 - 540 °F
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced
Data provided by Clariant Masterbatches
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant PA223 Nylon 6, Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 254 °C
490 °F
Teknor Apex Chemlon® 109-18 GH Nylon 66, 18% Glass Fiber Reinforced
Notes: High-impact; Reinforced with 18% glass fibers; Highly toughened compound designed to improve practical toughness and ductility Features: Ductile; Good Impact Resistance; Good Toughness; Good ..
Copyright © lookpolymers.com All Rights Reserved