PRODUCT NO. Category Trade Name
Rogers Corporation Bisco™ HT-1500 Solid Silicone Rubber Rubber or Thermoset Elastomer (TSE) Bisco™
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam Rubber or Thermoset Elastomer (TSE) Bisco™
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam Rubber or Thermoset Elastomer (TSE) Bisco™
Rogers Corporation Bisco™ RF-120 Cellular Silicone Foam Rubber or Thermoset Elastomer (TSE) Bisco™
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4701-50-15 Cellular Urethane Foam Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4701-60-20 Cellular Urethane Foam Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Handheld Urethane Foam, Handheld Grade, PET Reinforced Thermoset Polyurethane Foam, Unreinforced Poron® Shock Seal™
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Urethane Foam, Industrial Grade Thermoset Polyurethane Foam, Unreinforced Poron® Shock Seal™
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced Thermoset Polyurethane Foam, Unreinforced Poron® Shock Seal™
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam Thermoset Polyurethane Foam, Unreinforced Poron® ThinStik ShockSeal™
Rogers Corporation Poron® ThinStik Soft Seal 15-06021 Self-Adhesive Urethane Foam Thermoset Polyurethane Foam, Unreinforced Poron® ThinStik Soft Seal
Rogers Corporation Poron® ThinStik Soft Seal 15-06030 Self-Adhesive Urethane Foam Thermoset Polyurethane Foam, Unreinforced Poron® ThinStik Soft Seal
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam Thermoset Polyurethane Foam, Unreinforced Poron® ThinStik™
Rogers Corporation R/bak® SF Supported Firm Cushion Mounting Material Thermoset Polyurethane Foam, Unreinforced
Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft Thermoset Polyurethane Foam, Unreinforced
Rogers Corporation RO3010 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Rogers Corporation RO4003C Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil Ceramic Matrix Composite
Rogers Corporation RO4535 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate Thermoset
Rogers Corporation RO4835 Hydrocarbon Ceramic Laminate, Improved Oxidation Resistance Thermoset
Rogers Corporation RT/duroid® 6002 High Frequency Laminate Polymer
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate Polymer
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material Thermoplastic Syron™
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite Thermoset TMM®
Rogers Corporation XT/duroid™ 8000 Thermoplastic Laminate, Circuit Material Thermoplastic XT/duroid™
Rogers Corporation XT/duroid™ 8100 0.002" Woven Glass Reinforced Thermoplastic Circuit Material Thermoplastic XT/duroid™
Rogers Corporation Bisco® MF1 6535 - 35 Silicone, High Performance Foam, Indentation Force Material Silicone Foam Bisco®
Rogers Corporation Bisco™ FPC Cellular Silicone Foam Rubber or Thermoset Elastomer (TSE) Bisco™
Rogers Corporation Bisco™ HT-870 Cellular Silicone Foam Rubber or Thermoset Elastomer (TSE) Bisco™
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Thermoset Polyurethane Foam, Unreinforced Poron®
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film Fluoropolymer
Rogers Corporation Bisco® A2 R 1.5 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier Silicone, Molded, Glass Fiber Filled Bisco®
Rogers Corporation Bisco® A2 R 3.0 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier Silicone, Molded, Glass Fiber Filled Bisco®
Rogers Corporation Bisco® EC-2040 Conductive Silicone Silicone Bisco®
Rogers Corporation Bisco® L3 Premiere Next Generation Dynamic Flooring Material Silicone Foam Bisco®