Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Rogers Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow dielectric loss - high frequency performance can be used in applications exceeding 20 GHzLow in-plane expansion coefficient (match to copper) - suitable for use with epoxy multi-layer board hybrid designs and allows for more reliable surface mounted assembliesExcellent dimensional stability - high production yieldsEconomically priced - cost effective volume manufacturingSurface smoothness- allows for finer line etching tolerancesLead-free process compatibleUses:Automotive collision avoidance systemsAutomotive global positions satellite antennasWireless telecommunications systemsMicrostrip patch antennas for wireless communicationsDirect broadcast satellitesDatalink on cable systemsRemote meter readersPower backplanesLMDS and wireless broadbandBase station infrastructureInformation provided by Rogers Corporation.
Physical Properties Metric English Comments
Density 2.70 g/cc
0.0975 lb/in³
Water Absorption <= 0.10 %
<= 0.10 %
D24/23; IPC-TM-2.4.8
Thickness 635 - 1270 microns
25.0 - 50.0 mil
Range of Thicknesses Available
Mechanical Properties Metric English Comments
Tensile Modulus 3.19 GPa
462 ksi
MD; ASTM D638
3.19 GPa
462 ksi
TD; ASTM D638
Peel Strength 1.88 kN/m
10.7 pli
Copper; 1 oz. EDC After Solder Float; IPC-TM-650 2.4.8
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature -55.0 - 288 °C
7.22 µin/in-°F

@Temperature -67.0 - 550 °F
X, Y- Direction; ASTM D3386-94
34.0 µm/m-°C

@Temperature -55.0 - 288 °C
18.9 µin/in-°F

@Temperature -67.0 - 550 °F
Z-Direction; ASTM D3386-94
Specific Heat Capacity 0.850 J/g-°C
0.203 BTU/lb-°F
Calculated
Thermal Conductivity 0.670 W/m-K

@Temperature 80.0 °C
4.65 BTU-in/hr-ft²-°F

@Temperature 176 °F
ASTM C518
Decomposition Temperature 500 °C
932 °F
TGA; ASTM D3850
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Cond. A; IPC 2.5.17.1
Surface Resistance 1.00e+9 ohm
1.00e+9 ohm
Cond. A; IPC 2.5.17.1
Dielectric Constant 6.0 - 6.3

@Frequency 1.00e+10 Hz
6.0 - 6.3

@Frequency 1.00e+10 Hz
Clamped stripline, Z-direction; IPC-TM-650 2.5.5.5
6.6

@Frequency 8.00e+9 - 4.00e+10 Hz
6.6

@Frequency 8.00e+9 - 4.00e+10 Hz
Differential Phase Length Method, Z-Direction
Dissipation Factor 0.0027

@Frequency 1.00e+10 Hz
0.0027

@Frequency 1.00e+10 Hz
IPC-TM-650 2.5.5.5
Descriptive Properties Value Comments
Dimensional Stability 0.8 mm/m
ASTM D257, Cond. A; X, Y-direction
Thermal Coefficient of Dielectric Constant -212 ppm/°C
IPC-TM-650 2.5.5.5; 10 GHz; 0°C to 100°C; Z-Direction