Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Rogers Corporation Bisco® EC-2130 Conductive Silicone

Category Polymer , Thermoset , Silicone
Manufacturer Rogers Corporation
Trade Name Bisco®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rogers Corporation Bisco® EC-2130 Conductive Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.063 inches and 0.125 inchesInformation provided by Rogers Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.97 g/cc
1.97 g/cc
Thickness 1600 - 3180 microns
63.0 - 125 mil
Range of Thicknesses Available
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
ASTM D2240
Hardness, Shore OO 80
80
ASTM D2240
Tensile Strength >= 0.345 MPa
>= 50.0 psi
ASTM D142
Elongation at Break <= 50 %
<= 50 %
ASTM D412
Compression Set 5.0 %

@Temperature 70.0 °C
5.0 %

@Temperature 158 °F
% of thickness; ASTM D3574
7.0 %

@Temperature 100 °C
7.0 %

@Temperature 212 °F
% of thickness; ASTM D395 Method B
17 %

@Temperature 70.0 °C
17 %

@Temperature 158 °F
% of deflection; ASTM D3574
25 %

@Temperature 100 °C
25 %

@Temperature 212 °F
% of deflection; ASTM D395 Method B
Electrical Properties Metric English Comments
Volume Resistivity 0.30 ohm-cm
0.30 ohm-cm
Rogers Corp. Internal
Shielding Effectiveness 85 dB

@Thickness 1.60 mm,
Frequency 1.00e+10 Hz
85 dB

@Thickness 0.0630 in,
Frequency 1.00e+10 Hz
MIL G83528
100 dB

@Thickness 1.60 mm,
Frequency 1.00e+8 Hz
100 dB

@Thickness 0.0630 in,
Frequency 1.00e+8 Hz
MIL G83528
100 dB

@Thickness 1.60 mm,
Frequency 5.00e+8 Hz
100 dB

@Thickness 0.0630 in,
Frequency 5.00e+8 Hz
MIL G83528
110 dB

@Thickness 1.60 mm,
Frequency 1.00e+9 Hz
110 dB

@Thickness 0.0630 in,
Frequency 1.00e+9 Hz
MIL G83528
Users viewing this material also viewed the following: