Rogers Corporation Bisco® BF-2000 Ultra-Soft Silicone Foam

Category Polymer , Thermoset , Silicone , Silicone Foam
Manufacturer Rogers Corporation
Trade Name Bisco®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Rogers Corporation Bisco® BF-2000 Ultra-Soft Silicone Foam.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BISCO® Ultra Soft is a highly compressible silicone foam. The combination of low weight and softness makes this flame retardant foam ideal for transportation, industrial and electronics applications where low closure force and dust sealing are critical. Available in various thicknesses and manufactured in roll form.Features and Benefits:Ultra low softness allows designers to use less force to seal enclosures and still protect their device from the environment.High compressibility allows material to conform to variable width gaps, thereby allowing more design flexibility.Excellent memory and low stress relaxation reduces maintenance costs associated with gasket failures due to compression set and softening.Resistance to ultraviolet light, ozone, extreme temperatures and flame enables consistent performance in all environments.Color: blackThickness: 0.125 in to 0.500 inStandard Width: 0.500 in to 36.0 inApplications:Vibration isolation in electronic components and transportation vehiclesLow closure force gaskets within portable electronics such as laptops and LCD screens within aircraft and rail interiorsFire retardant thermal insulationInformation provided by Rogers Corporation.
Physical Properties Metric English Comments
Density 0.160 g/cc
0.00579 lb/in³
ASTM D1056
Thickness 3180 - 12700 microns
125 - 500 mil
Range of Thicknesses Available
Mechanical Properties Metric English Comments
Tensile Strength 0.172 MPa
25.0 psi
ASTM D412
Elongation at Break 80 %
80 %
ASTM D412
Compressive Yield Strength 0.0103 MPa
<br>@Strain 25.0 %
1.50 psi
<br>@Strain 25.0 %
ASTM D1056
Compression Set 1.0 %
<br>@Temperature 70.0 °C,<br> Time 79200 sec
1.0 %
<br>@Temperature 158 °F,<br> Time 22.0 hour
ASTM D1056
5.0 %
<br>@Temperature 100 °C,<br> Time 79200 sec
5.0 %
<br>@Temperature 212 °F,<br> Time 22.0 hour
ASTM D1056
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
also HF-1
Flame Spread Index <= 25
<= 25
I&lt;sub&gt;s&lt;/sub&gt;; ASTM E162
Smoke Density 1.5 min
1.5 min
&lt;20; D&lt;sub&gt;s&lt;/sub&gt;; ASTM E662
4.0 min
4.0 min
&lt;50; D&lt;sub&gt;s&lt;/sub&gt;; ASTM E662
Descriptive Properties Value Comments
Toxic Gas Emissions Pass
SMP-800C