| Polymer Resources ABS-FR Flame Retardant ABS |
Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant |
|
| Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized |
Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant |
|
| Polymer Resources ABS-FR1 ABS, Flame Retardant |
Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant |
|
| Polymer Resources ABS-G10 ABS, 10% Glass Reinforced |
Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled |
|
| Polymer Resources ABS-G30 ABS, 30% Glass Reinforced |
Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled |
|
| Polymer Resources ABS-G5 ABS, 5% Glass Reinforced |
Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled |
|
| Polymer Resources ABS-G5-[color]-3 ABS, 5% Glass Reinforced, UV-stabilized |
Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled |
|
| Polymer Resources ABS-GP1 General Purpose ABS |
Acrylonitrile Butadiene Styrene (ABS), Molded |
|
| Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized |
Acrylonitrile Butadiene Styrene (ABS), Molded |
|
| Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade |
Acrylonitrile Butadiene Styrene (ABS), Plating Grade |
|
| Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized |
Acrylonitrile Butadiene Styrene (ABS), Molded |
|
| Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified |
Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded |
|
| Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength |
Acetal Copolymer, Unreinforced |
|
| Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow |
Acetal Copolymer, Unreinforced |
|
| Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized |
Acetal Copolymer, Unreinforced |
|
| Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE |
Acetal Copolymer, PTFE Filled |
|
| Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized |
Acetal Copolymer, Unreinforced |
|
| Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized |
Acetal Homopolymer, Unreinforced |
|
| Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized |
Acetal Homopolymer, Unreinforced |
|
| Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized |
Acetal Homopolymer, Unreinforced |
|
| Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized |
Acetal Homopolymer, Unreinforced |
|
| Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE |
Acetal Homopolymer, PTFE-Filled |
|
| Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized |
Acetal Homopolymer, Unreinforced |
|
| Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized |
Acetal Homopolymer, Unreinforced |
|
| Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced |
Nylon 612, Glass Fiber Filler |
|
| Polymer Resources NY6/12-G43 Nylon 612, 43% Glass Reinforced |
Nylon 612, Glass Fiber Filler |
|
| Polymer Resources NY6/12-GP1 General Purpose Nylon 612 |
Nylon 612, Unreinforced |
|
| Polymer Resources NY66-EX1 High Viscosity Nylon 66 |
Nylon 66, Extruded |
|
| Polymer Resources NY66-FRG25 Flame Retardant Nylon 66, 25% Glass Reinforced |
Nylon 66, Glass Fiber Filled, Flame Retardant |
|
| Polymer Resources NY66-G13 Nylon 66, 13% Glass Reinforced |
Nylon 66, 10% Glass Fiber Filled |
|
| Polymer Resources NY66-G20-MD Nylon 66, 20% Glass Reinforced with MoS2 |
Nylon 66, MoS2 Filled |
|
| Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced |
Nylon 66, 30% Glass Fiber Filled |
|
| Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) |
Nylon 66, 30% Glass Fiber Filled |
|
| Polymer Resources NY66-G43 Nylon 66, 43% Glass Reinforced |
Nylon 66, 40% Glass Fiber Filled |
|
| Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized |
Nylon 66, 40% Glass Fiber Filled |
|
| Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced |
Nylon 66, 50% Glass Fiber Filled |
|
| Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced |
Nylon 66, 60% Glass Fiber Filled |
|
| Polymer Resources NY66-GP1 General Purpose Nylon 66 |
Nylon 66, Unreinforced |
|
| Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized |
Nylon 66, Unreinforced |
|
| Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM) |
Nylon 66, Heat Stabilized |
|
| Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized |
Nylon 66, Unreinforced |
|
| Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened |
Nylon 66, 10% Glass Fiber Filled |
|
| Polymer Resources NY66-IM1-G33-[color]-H Nylon 66, 33% Glass Reinforced, Toughened and Heat Stabilized |
Nylon 66, Heat Stabilized |
|
| Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized |
Nylon 66, Heat Stabilized |
|
| Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM) |
Nylon 66, Impact Grade |
|
| Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified |
Nylon 66, 10% Glass Fiber Filled |
|
| Polymer Resources NY66-IM2-G13-[color]-H Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized |
Nylon 66, 10% Glass Fiber Filled |
|
| Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified |
Nylon 66, 30% Glass Fiber Filled |
|
| Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized |
Nylon 66, 30% Glass Fiber Filled |
|
| Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM) |
Nylon 66, Impact Grade |
|
| Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) |
Nylon 66, 10% Glass Fiber Filled |
|
| Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM) |
Nylon 66, 30% Glass Fiber Filled |
|
| Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified |
Nylon 66, 40% Glass Fiber Filled |
|
| Polymer Resources NY66-M25G15 Nylon 66, 25% Mineral, 15% Glass Reinforced |
Nylon 66, Glass/Mineral Filled |
|
| Polymer Resources NY66-M25G15-[color]-H Nylon 66, 25% Mineral, 15% Glass Reinforced, Heat Stabilized |
Nylon 66, Glass/Mineral Filled |
|
| Polymer Resources NY66-M40 Nylon 66, 40% Mineral Filled |
Nylon 66, 40% Mineral Filled |
|
| Polymer Resources NY66-M40-[color]-H Nylon 66, 40% Mineral Filled, Heat Stabilized |
Nylon 66, 40% Mineral Filled |
|
| Polymer Resources NY66-MD-[color]-H Nylon 66, 2% MoS2 |
Nylon 66, MoS2 Filled |
|
| Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM) |
Nylon 66, MoS2 Filled |
|
| Polymer Resources NY66-MD1 Nylon 66, 1% MoS2 |
Nylon 66, MoS2 Filled |
|
| Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced |
Nylon 6, 10% Glass Fiber Filled |
|
| Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) |
Nylon 6, 20% Glass Fiber Filled |
|
| Polymer Resources NY6-G20 Nylon 6, 20% Glass Reinforced |
Nylon 6, 20% Glass Fiber Filled |
|
| Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced |
Nylon 6, 30% Glass Fiber Filled |
|
| Polymer Resources NY6-G33 Nylon 6, 33% Glass Reinforced |
Nylon 6, 30% Glass Fiber Filled |
|
| Polymer Resources NY6-G33-[color]-H Nylon 6, 33% Glass Reinforced, Heat Stabilized |
Nylon 6, 30% Glass Fiber Filled |
|
| Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) |
Nylon 6, 30% Glass Fiber Filled |
|
| Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced |
Nylon 6, 40% Glass Fiber Filled |
|
| Polymer Resources NY6-G50 Nylon 6, 50% Glass Reinforced |
Nylon 6, 50% Glass Fiber Filled |
|
| Polymer Resources NY6-GP1 General Purpose Nylon 6 |
Nylon 6, Unreinforced |
|
| Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized |
Nylon 6, Unreinforced |
|
| Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM) |
Nylon 6, Heat Stabilized |
|
| Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated |
Nylon 6, Unreinforced |
|
| Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized |
Polycarbonate/Thermoplastic Polyurethane Blend |
|
| Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled |
Polycarbonate/ABS Alloy, Glass Fiber Filled |
|
| Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled |
Polycarbonate/ABS Alloy, Glass Fiber Filled |
|
| Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy |
ASA Polymer |
|
| Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP2 PC/Polyester Alloy |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP2-G10 PC/Polyester Alloy, 10% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding |
Polycarbonate, Extruded |
|
| Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized |
Polycarbonate, Extruded |
|
| Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant |
Polycarbonate, Gamma Radiation Resistant |
|
| Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant |
Polycarbonate, Gamma Radiation Resistant |
|