| Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized |
Polycarbonate/Thermoplastic Polyurethane Blend |
|
| Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled |
Polycarbonate/ABS Alloy, Glass Fiber Filled |
|
| Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled |
Polycarbonate/ABS Alloy, Glass Fiber Filled |
|
| Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy |
ASA Polymer |
|
| Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP2 PC/Polyester Alloy |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC/TP-GP2-G10 PC/Polyester Alloy, 10% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced |
Polycarbonate/PET Polyester Blend, Glass Reinforced |
|
| Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified |
Polycarbonate/PET Polyester Blend |
|
| Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding |
Polycarbonate, Extruded |
|
| Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized |
Polycarbonate, Extruded |
|
| Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant |
Polycarbonate, Gamma Radiation Resistant |
|
| Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant |
Polycarbonate, Gamma Radiation Resistant |
|
| Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant |
Polycarbonate, Gamma Radiation Resistant |
|
| Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant |
Polycarbonate, Gamma Radiation Resistant |
|
| Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant |
Polycarbonate, Gamma Radiation Resistant |
|
| Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE |
Polycarbonate, PTFE Filled |
|
| Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant |
Polycarbonate, Unreinforced, Flame Retardant |
|
| Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow |
Polycarbonate, PTFE Filled |
|
| Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced |
Polycarbonate, 10% Glass Filled |
|
| Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release |
Polycarbonate, 10% Glass Filled |
|
| Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified |
Polycarbonate, Impact Modified |
|
| Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced |
Polycarbonate, 20% Glass Filled |
|
| Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced |
Polycarbonate, 20% Glass Filled |
|
| Polymer Resources PC-G20-[color]-1 Polycarbonate, 20% Glass Reinforced with Mold Release |
Polycarbonate, 20% Glass Filled |
|
| Polymer Resources PC-G20-[color]-WS Polycarbonate, 20% Glass Reinforced |
Polycarbonate, 20% Glass Filled |
|
| Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced |
Polycarbonate, 30% Glass Filled |
|
| Polymer Resources PC-G30-TFE15 Polycarbonate, 30% Glass Reinforced, 15% PTFE |
Polycarbonate, Glass + PTFE Filled |
|
| Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced |
Polycarbonate, 40% Glass Filled |
|
| Polymer Resources PC-G40-[color]-1 Polycarbonate, 40% Glass Reinforced with Mold Release |
Polycarbonate, 40% Glass Filled |
|
| Polymer Resources PC-G5-IM Polycarbonate, 5% Glass Reinforced, Impact Modified, Foamable |
Polycarbonate, Foam Grade, Glass Filled |
|
| Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP1-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow |
Polycarbonate, PTFE Filled |
|
| Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP2-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Medium Flow |
Polycarbonate, PTFE Filled |
|
| Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP3-TFE10 Polycarbonate, 10% PTFE, High Flow, Wear Resistant |
Polycarbonate, PTFE Filled |
|
| Polymer Resources PC-GP3-TFE5 Polycarbonate, 5% PTFE, High Flow, Wear Resistant |
Polycarbonate, PTFE Filled |
|
| Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP4-[color]-3 Polycarbonate, UV-stabilized, Easy Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP4-[color]-4 Polycarbonate, UV-stabilized, Easy Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC-HH Polycarbonate, High Heat |
Polycarbonate, High Heat |
|
| Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized |
Polycarbonate, High Heat |
|
| Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant |
Polycarbonate, 10% Glass Filled |
|
| Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release |
Polycarbonate, 10% Glass Filled |
|
| Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized |
Polycarbonate, 10% Glass Filled |
|
| Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release |
Polycarbonate, 10% Glass Filled |
|
| Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release |
Polycarbonate, 10% Glass Filled |
|
| Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release |
Polycarbonate, 10% Glass Filled |
|
| Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow |
Polycarbonate, Impact Modified |
|
| Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized |
Polycarbonate, Impact Modified |
|
| Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow |
Polycarbonate, Impact Modified |
|
| Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized |
Polycarbonate, Impact Modified |
|
| Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow |
Polycarbonate, Impact Modified |
|
| Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow |
Polycarbonate, Impact Modified |
|
| Polymer Resources PCSF-FR G30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade |
Polycarbonate, Foam Grade, Glass Filled |
|
| Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade |
Polycarbonate, Foam Grade, Glass Filled |
|
| Polymer Resources PCSF-FRG30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade |
Polycarbonate, Foam Grade, Glass Filled |
|
| Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow |
Polycarbonate, Molded |
|
| Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release |
Polycarbonate, Molded |
|
| Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized |
Polycarbonate/ABS Alloy, Unreinforced |
|
| Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled |
Polycarbonate/ABS Alloy, Glass Fiber Filled |
|