| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
PlastiComp Complet® LCF50 - PA6 Nylon 6, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
PlastiComp Complet® LGF30 - PA6 Nylon 6, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
|
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced
Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
|
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
|
|||
| Melt Temperature | 260 - 288 °C | 500 - 550 °F | Air purge at equilibrium conditions |
|
NOVA Chemicals Dylark® 480P12 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
|
|||
| Melt Temperature | 249 - 288 °C | 480 - 550 °F | |
|
Huntsman PE5082 Extrusion Coating Polyethylene
(discontinued **)
Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings (sugar paper and laminations).FDA Notes: Con..
|
|||
| Melt Temperature | 260 - 288 °C | 500 - 550 °F | Air purge at equilibrium conditions |
|
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
|
|||
| Melt Temperature | 260 - 288 °C | 500 - 550 °F | Air purge at equilibrium conditions |
|
NOVA Chemicals Dylark® 480P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)
(discontinued **)
Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically..
|
|||
| Melt Temperature | 238 - 288 °C | 460 - 550 °F | |
|
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin
(discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||
| Melt Temperature | 224 - 288 °C | 435 - 550 °F | Average value: 256 °C Grade Count:5 |
|
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ..
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Entec Hylex® P1017FR Polycarbonate
Information provided by Ravago.
|
|||
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
|
Entec Hylex® P1317FR Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol 6601FR Nylon 66, Flame Retardant
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol PA101F/ST801 Nylon 66, Impact Modified, Lubricated
Data provided by Clariant Masterbatches
|
|||