| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
| Water Absorption | 1.1 % | 1.1 % | 24 hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | 0.125 in; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 121 | 121 | ASTM D785 |
| Tensile Strength, Yield | 193 MPa | 28000 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Flexural Strength | 276 MPa | 40000 psi | ASTM D790 |
| Flexural Modulus | 9.45 GPa | 1370 ksi | ASTM D790 |
| Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | 73°F; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | HB | HB | 0.0590 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
| Drying Temperature | 73.9 °C | 165 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
| Moisture Content | 0.18 % | 0.18 % | |
| Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
| Screw Speed | 50 - 120 rpm | 50 - 120 rpm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure | 750 to 1400 psi | |
| Injection Rate | Fast |