| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Therma-Tech™ NJ-6000 TC Polyamide 12 (Nylon 12) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-100-BU03 Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-100-BW01 Natural PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-100-CX01 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-500-CX01 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-500-CX02 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
| Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
| Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Electrical Properties, High Heat and Chemical ResistanceApplications: Connectors, Relays, Switches, Automotive (Under Hood), AppliancesProcessing: Injection Molding.. |
|||
| Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
| Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat.. |
|||
| Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
| Covestro Petlon® DP3-1027 Semi-Crystalline PET, 45% Glass Fiber
(discontinued **) Characteristics: General Purpose: Good Strength, High Rigidity and Heat ResistanceApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperature: 4.. |
|||
| Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
| Covestro Petlon® DP3-1039 Semi-Crystalline PET, 35% Glass Fiber
(discontinued **) Characteristics: Impact Modified: Good Strength and ToughnessApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperature: 495-530°F, Mold Tempe.. |
|||
| Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
| Covestro Petlon® DP3-1042 Semi-Crystalline PET, 40% Mineral/Glass Fiber
(discontinued **) Characteristics: General Purpose: Good Strength and Dimensional Stability, Low WarpageApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperatur.. |
|||
| Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
| Covestro Petlon® 4835 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
| Melt Temperature | 210 - 277 °C | 410 - 531 °F | Average value: 260 °C Grade Count:19 |
| Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
| Melt Temperature | 246 - 277 °C | 475 - 531 °F | Average value: 262 °C Grade Count:5 |
| Overview of materials for Polycarbonate/Styrenic Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| Styron EMERGEâ„¢ 4310-22 Polycarbonate EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| Styron EMERGEâ„¢ 4330-22 Polycarbonate EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| Styron EMERGEâ„¢ 4850-19 Polycarbonate EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| Styron EMERGEâ„¢ 4800-19 Polycarbonate EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
| Melt Temperature | 232 - 277 °C | 450 - 531 °F | |
| Eastman DuraStar MN611 Polymer, Natural Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
| Melt Temperature | 20.0 - 277 °C | 68.0 - 531 °F | Average value: 246 °C Grade Count:16 |
| Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
| Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
| Covestro Petlon® 3530 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Underhood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperatu.. |
|||
| Melt Temperature | 254 - 277 °C | 489 - 531 °F | |
| PolyOne Stat-Tech™ NJ-20CF/000 Black Polyamide 12 (Nylon 12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-100-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-100-CX02-EG PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
| Melt Temperature | 260 - 277 °C | 500 - 531 °F | |
| PolyOne Edgetek® XT XT-500-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||