Category Polymer , Film , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon 6. It possesses the combination of strength, toughness and thermo-forming properties associated with nylon 6 as well as excellent heat, chemical, and abrasion resistance.Applications:Processed MeatFresh Red MeatPoultryFishCheeseDried FoodChilled Fruit JuicesInformation provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D1505
Water Absorption 0.80 %
0.80 %
Extractable Content
1.6 %
1.6 %
in 24 hours
Moisture Absorption at Equilibrium 2.7 %
2.7 %
at 50% RH
Water Absorption at Saturation 9.5 %
9.5 %
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm
35.6 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm
185 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Viscosity Measurement 135
135
FAV; ASTM D789
Maximum Moisture Content 0.080
0.080
Melt Flow 1.2 g/10 min

@Load 1.00 kg,
Temperature 235 °C
1.2 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
Processing Properties Metric English Comments
Middle Barrel Temperature 230 - 260 °C
446 - 500 °F
Cast Film
246 - 254 °C
475 - 489 °F
Tubular (Blown) Film
Adapter Temperature 260 °C
500 °F
Tubular (Blown) Film
260 - 266 °C
500 - 511 °F
Cast Film
Die Temperature 254 °C
490 °F
Tubular (Blown) Film
260 °C
500 °F
Cast Film
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
260 - 270 °C
500 - 518 °F
Cast Film
Moisture Content 0.080 %