Kostat G148BK TAB Spacer Reels

Category Polymer , Thermoplastic
Manufacturer Kostat
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kostat G148BK TAB Spacer Reels.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
KOSTATs TAB Spacer Reels are ideal for shipment and storage of any components packaged in TAB spacer tapes. KOSTATSs TAB Spacer Reels, uniquely formulated and manufactured with the most advanced injection molding technology, are made of ABS compound with IDP alloy technology. This class of materials has distinctive advantages in ESD properties, providing permanent static dissipation. Also, this product exhibits superior cleanliness performance compared with other competitive antistatic and conductive thermoplastic materials.Special Features:Superior Permanent Static DissipationHumidity InsensitivityExcellent Wear resistanceLow Particle GenerationExcellent Warpage ResistanceReusabilitySimple Easy to use Locking SystemModular Design Requiring Less Storage SpaceApplications:Semiconductors PackagingLCD Components PackagingHDD Components PackagingElectrical & Electronics PackagingMedical Devices PackagingClean Room Accessories
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
ASTM D638
Flexural Strength 59.0 MPa
8560 psi
ASTM D790
Flexural Modulus 4.60 GPa
667 ksi
ASTM D790
Izod Impact, Notched 0.330 J/cm
0.618 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+10 ohm
1.00e+10 ohm
ASTM D257
Static Decay <= 0.50 sec
<= 0.50 sec
5kV to 50V; FTMS 101C
Processing Properties Metric English Comments
Drying Temperature 80.0 - 90.0 °C
176 - 194 °F
Dry Time 3 - 4 hour
3 - 4 hour