| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergamid™ PA66 C20 Black Polyamide 66 (Nylon 66).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 203 MPa @Temperature 23.0 °C |
29400 psi @Temperature 73.4 °F |
ISO 527 |
| Elongation at Break | 2.3 % @Temperature 23.0 °C |
2.3 % @Temperature 73.4 °F |
ISO 527 |
| Tensile Modulus | 13.2 GPa @Temperature 23.0 °C |
1910 ksi @Temperature 73.4 °F |
ISO 527 |
| Charpy Impact Unnotched | 6.10 J/cm² @Temperature 23.0 °C |
29.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Unannealed; ISO 75-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 235 °C | 455 °F | Unannealed; ISO 75-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1700 ohm | 1700 ohm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
| Mold Temperature | 65.0 - 85.0 °C | 149 - 185 °F | |
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Black | |
| Features | Good Dimensional Stability | |
| Good Impact Resistance | ||
| Good Stiffness | ||
| Filler / Reinforcement | Carbon Fiber Reinforcement, 20% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | Nylon 66 | |
| Generic Name | Polyamide 66 (Nylon 66) | |
| Processing Method | Injection Molding | |
| Regional Availability | Asia Pacific | |
| Europe | ||
| North America |