| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer |
| Manufacturer | LG Chemical |
| Trade Name | KEYFLEX |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical KEYFLEX BT 1033D Ester Type TPE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
| Water Absorption | 0.70 % <br>@Temperature 23.0 °C,<br> Time 86400 sec |
0.70 % <br>@Temperature 73.4 °F,<br> Time 24.0 hour |
ASTM D570 |
| Molecular Weight | 458.458 g/mol | 458.458 g/mol | |
| Maximum Moisture Content | 0.010 | 0.010 | Injection Molding |
| 0.010 | 0.010 | Extrusion Molding | |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm <br>@Thickness 3.20 mm |
0.0040 - 0.0080 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 25 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
25 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 85 | 85 | ASTM D2240 |
| Hardness, Shore D | 31 | 31 | ASTM D2240 |
| Tensile Strength at Break | 23.5 MPa <br>@Thickness 2.00 mm |
3410 psi <br>@Thickness 0.0787 in |
50mm/min; ASTM D638 |
| Elongation at Break | 800 % <br>@Thickness 2.00 mm |
800 % <br>@Thickness 0.0787 in |
50mm/min; ASTM D638 |
| Izod Impact, Notched | NB <br>@Thickness 6.40 mm,<br> Temperature 23.0 °C |
NB <br>@Thickness 0.252 in,<br> Temperature 73.4 °F |
ASTM D256 |
| NB <br>@Thickness 6.40 mm,<br> Temperature -40.0 °C |
NB <br>@Thickness 0.252 in,<br> Temperature -40.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 185 °C | 365 °F | Peak |
| Boiling Point | 140 - 230 °C | 284 - 446 °F | |
| Flash Point | 300 - 340 °C | 572 - 644 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 600 V | 600 V | Solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 185 - 205 °C | 365 - 401 °F | Injection Molding |
| Middle Barrel Temperature | 195 - 215 °C | 383 - 419 °F | Injection Molding |
| Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
| Zone 1 | 185 - 205 °C | 365 - 401 °F | Extrusion Molding |
| Zone 2 | 195 - 215 °C | 383 - 419 °F | Extrusion Molding |
| Zone 3 | 195 - 215 °C | 383 - 419 °F | Extrusion Molding |
| Zone 4 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
| Adapter Temperature | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
| Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion Molding |
| Melt Temperature | 185 - 225 °C | 365 - 437 °F | Injection Molding |
| 185 - 225 °C | 365 - 437 °F | Extrusion Molding | |
| Mold Temperature | 10.0 - 35.0 °C | 50.0 - 95.0 °F | Injection Molding |
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
| 80.0 - 90.0 °C | 176 - 194 °F | Extrusion Molding | |
| Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
| 3.00 - 4.00 hour | 3.00 - 4.00 hour | Extrusion Molding |