Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latistat 47/7-03 PP Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer LATI
Trade Name Latistat
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latistat 47/7-03 PP Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dissipative product based on Polypropylene copolymer (PPc). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
Linear Mold Shrinkage, Transverse 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
Elongation at Break 7.0 %
7.0 %
Elongation at Yield 5.0 %
5.0 %
Tensile Modulus 2.10 GPa
305 ksi
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 80 ohm
80 ohm
Processing Properties Metric English Comments
Melt Temperature 200 - 240 °C
392 - 464 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: