Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
Rear Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced Modified-Polyphenylene Oxide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Rear Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Rear Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUMID HI2152A(W) PA6+GF15%, High Impact Feature: Injection Molding, PA6+GF15%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical LUMID SG2460B PA66+GF46%, General purpose, Good Surface Feature: Injection Molding, PA66+GF46%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base PlateCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical LUPOY SC5004T PC/Polyester, Transparency Description: Injection Molding, PC/Polyester, General Purpose, Transparency, High FlowApplication: Keypad for Mobile PhoneCAS: 103598-77-2Information provided by LG Chemical |
|||
Rear Barrel Temperature | 260 - 293 °C | 500 - 560 °F | |
LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled 33% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 260 - 300 °C | 500 - 572 °F | Injection Molding |
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9 and 181028.. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUPOY GP1006FL PC, Flame Retardant Description: Injection Molding, PC, Flame Retardant, High FlowApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Rear Barrel Temperature | 260 °C | 500 °F | |
MTI ThermoStran® PA66-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Teknor Apex Beetle® PET166F Polyethylene Terephthalate, 30% Glass Fiber Reinforced Notes: PET166F is a 30% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperature and excellent mold release. Processing Method: Injection Molding Forms: Pe.. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Unitika C300VN Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 66 UNR Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Unitika FUN-8000 Characteristics: High impact strength High chemical resistance Transparency as high as polycarbonateInformation provided by Unitika Ltd. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Rear Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |