| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 266 - 271 °C | 510 - 520 °F | |
|
Polymer Resources NY66-EX1 High Viscosity Nylon 66
Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as ..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow
High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized
High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced
Superior Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow
Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release
Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow
Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Rear Barrel Temperature | 221 - 271 °C | 430 - 520 °F | |
|
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
|
|||
| Rear Barrel Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced
Information provided by Ravago.
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)&
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC/TP-GP1 PC/Polyester Alloy
High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow
Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
MRC Polymers EMAREXâ„¢ 300 GF33 Nylon 6, 33% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy
Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati..
|
|||
| Rear Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
|
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
|
|||
| Rear Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
|
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release
Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package ..
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity
Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc.
|
|||
| Rear Barrel Temperature | 243 - 271 °C | 470 - 520 °F | |
|
Star Plastics PC/PBT7820 Molding Grade PC/PBT
Information provided by Star Plastics, Inc.
|
|||
| Rear Barrel Temperature | 243 - 271 °C | 470 - 520 °F | |
|
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT
Information provided by Star Plastics, Inc.
|
|||
| Rear Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 221 - 271 °C | 430 - 520 °F | |
|
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced
(Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||