| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 290 - 300 °C | 554 - 572 °F | |
|
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu
Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu..
|
|||
| Rear Barrel Temperature | 290 - 300 °C | 554 - 572 °F | |
|
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **)
Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical..
|
|||
| Rear Barrel Temperature | 260 - 300 °C | 500 - 572 °F | |
|
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
|
|||
| Rear Barrel Temperature | 260 - 300 °C | 500 - 572 °F | Injection Molding |
|
LG Chemical LUCON CP6052 PC/ABS+CNT
Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, Low Surface Resistivity, Improved Impact StrengthApplication: Laser diode Tray, ATM parts, Telecommunication Station Housi..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | Injection Molding |
|
LG Chemical LUCON CP6062EX PC/ABS+CNT
Description: Sheet Extrusion or Injection Molding, PC/ABS+CNT, Electrostatic Dissipation, Wide Processing Range, Low Surface ResistivityApplication: BLU Carrying TrayCAS No. 103598-77-2, 9003-56-9, ..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | Injection Molding |
|
LG Chemical LUCON CP6080LP PC+CNT+GF
Description: Injection Molding, PC+CNT+GF, Electrostatic Dissipation, Low Surface TribochargeApplication: ATM parts, HDD BracketCAS No. 103598-77-2, 65997-17-3 and 7782-42-5Information provided by L..
|
|||
| Rear Barrel Temperature | 260 - 300 °C | 500 - 572 °F | Injection Molding |
|
LG Chemical LUCON SP9306FL sPS+MF
Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 ..
|
|||
| Rear Barrel Temperature | 260 - 300 °C | 500 - 572 °F | |
|
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE
NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co..
|
|||
| Rear Barrel Temperature | 270 - 300 °C | 518 - 572 °F | Injection Molding |
|
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi..
|
|||
| Rear Barrel Temperature | 270 - 300 °C | 518 - 572 °F | Injection Molding |
|
LG Chemical LUPOY GP2300 PC+GF30%, Heat Resistance
Description: Injection Molding, PC+GF30%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
|
|||
| Rear Barrel Temperature | 270 - 300 °C | 518 - 572 °F | |
|
LG Chemical LUPOY GP-2301F General Purpose Modified PC, 30% Glass Fiber Reinforced, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Rear Barrel Temperature | 270 - 300 °C | 518 - 572 °F | |
|
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Rear Barrel Temperature | 270 - 300 °C | 518 - 572 °F | |
|
LG Chemical LUPOY GP-2401F General Purpose Modified PC, 40% Glass Fiber Reinforced, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Rear Barrel Temperature | 270 - 300 °C | 518 - 572 °F | Injection Molding |
|
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
|
|||
| Rear Barrel Temperature | 260 - 300 °C | 500 - 572 °F | Injection Molding |
|
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9 and 181028..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Samyang Trirex® 3022A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Samyang Trirex® 3025G10 Polycarbonate, 10% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Samyang Trirex® 3027IR Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Samyang Trirex® 3030I Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Samyang Trirex® 3030IR Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Samyang Trirex® 3030U Polycarbonate, UV Stabilized
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Samyang Trirex® 3500G30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr..
|
|||
| Rear Barrel Temperature | 270 - 300 °C | 518 - 572 °F | Injection Molding |
|
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance
Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | Injection Molding |
|
LG Chemical LUXY KS G55 Amorphous PA6
Description: Injection Molding, Amorphous PA6, High Modulus, High Impact, Low WarpageApplication: Electric/Electronic Components (LCD Bracket)Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 260 - 300 °C | 500 - 572 °F | |
|
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
|
|||
| Rear Barrel Temperature | 280 - 300 °C | 536 - 572 °F | Injection Molding |
|
LG Chemical LUCON CP6067 PC+CNT+CF
Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74..
|
|||