| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled |
| Manufacturer | LG Chemical |
| Trade Name | LUMID |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical LUMID SG2460B PA66+GF46%, General purpose, Good Surface.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
| Water Absorption | 0.60 % | 0.60 % | ASTM D570 |
| Maximum Moisture Content | 0.090 | 0.090 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0030 - 0.0070 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength, Yield | 196 MPa <br>@Thickness 3.20 mm |
28400 psi <br>@Thickness 0.126 in |
5mm/min; ASTM D638 |
| Elongation at Break | 3.0 % <br>@Thickness 3.20 mm |
3.0 % <br>@Thickness 0.126 in |
5mm/min; ASTM D638 |
| Flexural Yield Strength | 275 MPa <br>@Thickness 3.20 mm |
39800 psi <br>@Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Flexural Modulus | 11.8 GPa <br>@Thickness 3.20 mm |
1710 ksi <br>@Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Izod Impact, Notched | 1.37 J/cm <br>@Thickness 6.40 mm,<br> Temperature 23.0 °C |
2.57 ft-lb/in <br>@Thickness 0.252 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
| Melting Point | 220 °C | 428 °F | ASTM D3418 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C <br>@Thickness 6.40 mm |
410 °F <br>@Thickness 0.252 in |
Unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Constant | 4.0 <br>@Frequency 1.00e+6 Hz |
4.0 <br>@Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 25.0 kV/mm <br>@Thickness 1.00 mm |
635 kV/in <br>@Thickness 0.0394 in |
ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
| Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
| Front Barrel Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
| Nozzle Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
| Melt Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
| Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | Injection Molding |
| Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
| Screw Speed | 30 - 60 rpm | 30 - 60 rpm | Injection Molding |