Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by.. |
|||
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by .. |
|||
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 60% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Rear Barrel Temperature | 260 - 299 °C | 500 - 570 °F | |
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-FR7 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 260F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP4 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-FRG20 Modified PPO, UL 94 V-1, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP1 Modified PPO, General Purpose with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP2 Modified PPO, General Purpose with HDT of 250 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 288 - 299 °C | 550 - 570 °F | |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 288 - 299 °C | 550 - 570 °F | |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LGF30 - PA66 Nylon 66, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LGF40 - PA66 Nylon 66, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Rear Barrel Temperature | 260 - 299 °C | 500 - 570 °F | |
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-FR7 Modified PPO, V-0 Flame Retardant, Medium Heat, 250 HDT
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-MF-FR3 Modified PPO, UL 94 V-0 with HDT of 230 F, Mineral Reinforced
(Unverified Da Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |