Processing Properties Metric English Comments
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow
Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow
Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t..
Rear Barrel Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources PC-G30-TFE15 Polycarbonate, 30% Glass Reinforced, 15% PTFE
Polycarbonate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact
Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, ..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow
Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release
Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow
Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-GP1-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release
Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-GP3-TFE5 Polycarbonate, 5% PTFE, High Flow, Wear Resistant
Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow
Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release
Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Rear Barrel Temperature 288 - 304 °C
550 - 580 °F
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 288 - 304 °C
550 - 579 °F
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement  (discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples...
Rear Barrel Temperature 288 - 304 °C
550 - 580 °F
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
LTL Color Compounds ColorFast® PC60 Polycarbonate
6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled
High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 288 - 304 °C
550 - 580 °F
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 288 - 304 °C
550 - 580 °F
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 288 - 304 °C
550 - 580 °F
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 288 - 299 °C
550 - 570 °F
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
Rear Barrel Temperature 288 - 288 °C
550 - 550 °F
Star Plastics PC703 Molding Grade PC with release
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC731 Molding Grade PC
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC733R Molding Grade PC
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PCGF10 Molding Grade PC with 10% Glass
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PCGF30 Molding Grade PC with 30% Glass
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
LTL Color Compounds ColorFast® FRPC310 Polycarbonate, Flame-Retarded
V0-rated 10% glass-filled polycarbonate, excellent impact strengthAll information provided by LTL Color Compounders, Inc.
Copyright © lookpolymers.com All Rights Reserved