Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 93.3 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 93.3 - 149 °C
200 - 300 °F
PolyOne LubriOne™ SF2-30CF/15T Natural Polyphenylene Sulfide (PPS)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Mold Temperature 93.3 °C
200 °F
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by..
Mold Temperature 93.3 °C
200 °F
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc.
Mold Temperature 93.3 - 121 °C
200 - 250 °F
PolyOne Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Mold Temperature 93.3 - 163 °C
200 - 325 °F
Oxford Polymers Oxtron PPS-XT-40GF PPS, 40% Glass Reinforced
Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy. Processing and Delivery Form: Pellets and Injection MoldingAppearance: Natural off-whit..
Mold Temperature 93.3 - 110 °C
200 - 230 °F
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced
Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
Mold Temperature 93.3 °C
200 °F
Northstar Polymers MSS-A70GQ High Performance Polyurethane Cast Elastomer System 70A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires cut/tear resistance, dry-abrasion resistance, slow resp..
Mold Temperature 93.3 - 121 °C
200 - 250 °F
PolyOne Lubri-Tech™ PS-30GF/02S Polybutylene Terephthalate (PBT), Glass Filled, PTFE/Silicone Lubricated  (dis
Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 93.3 - 121 °C
200 - 250 °F
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 93.3 - 107 °C
200 - 225 °F
PolyOne Edgetek® NL-43GF/000 Nylon 6/12, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 93.3 - 121 °C
200 - 250 °F
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced
Data provided by Clariant Masterbatches
Mold Temperature 93.3 - 121 °C
200 - 250 °F
Clariant Renol PA1SP0019 Nylon 66/PPS Alloy, 20% Glass, 20% Mineral
Data provided by Clariant Masterbatches
Mold Temperature 93.3 - 104 °C
200 - 220 °F
PolyOne Lubri-Tech™ NI-10CF/15T Nylon 6/10, Carbon Fiber Reinforced, PTFE Lubricated  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature >= 93.3 °C
>= 200 °F
PolyOne Edgetek® NI-20GF/000 Nylon 6/10, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 93.3 - 104 °C
200 - 220 °F
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated  (discontinue
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 93.3 - 149 °C
200 - 300 °F
PolyOne Edgetek® PF-40CF/000 Polysulfone, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 93.3 - 163 °C
200 - 325 °F
PolyOne Edgetek® RA-15GF/000 Polyethersulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0UL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 93.3 - 121 °C
200 - 250 °F
PolyOne Lubri-Tech™ MP-20CF/15T Modified Polyphenylene Oxide (mPPO), Carbon Fiber Reinforced, PTFE Lubricated  
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Copyright © lookpolymers.com All Rights Reserved