Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 93.3 - 107 °C | 200 - 225 °F | |
PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Mold Temperature | 93.3 °C | 200 °F | |
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Mold Temperature | 93.3 °C | 200 °F | |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Mold Temperature | 93.3 °C | 200 °F | |
Northstar Polymers MSS-A70GQ High Performance Polyurethane Cast Elastomer System 70A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires cut/tear resistance, dry-abrasion resistance, slow resp.. |
|||
Mold Temperature | 93.3 °C | 200 °F | |
PolyOne Edgetek® NI-10GF/000 Polyamide 610 (Nylon 610) Information provided by PolyOne |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
PolyOne Lubri-Tech™ PS-15GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
PolyOne Edgetek® PS-20GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 °C | 200 °F | |
PlastiComp Complet® LCF40 - PA6 Nylon 6, 40% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
LNP Thermocomp® FP-EC-1004 Ethylene Tetrafluoroethylene Copolymer, Carbon Fiber Reinforcement
(discontinued * Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Mold Temperature | 93.3 - 163 °C | 200 - 325 °F | Average value: 126 °C Grade Count:13 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Mold Temperature | 93.3 - 104 °C | 200 - 220 °F | |
PolyOne Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 °C | 200 °F | |
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Mold Temperature | >= 93.3 °C | >= 200 °F | |
PolyOne Edgetek® NI-20GF/000 Nylon 6/10, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
PolyOne Stat-Tech™ ES-06CF-09GF/000 Polyethersulfone, Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 - 149 °C | 200 - 300 °F | |
PolyOne Lubri-Tech™ PI-30GF/15T Polyetherimide (PEI), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |