Processing Properties Metric English Comments
Mold Temperature 49.0 - 66.0 °C
120 - 151 °F
PolyOne Lubri-Tech™ AS-000/10T-2S ABS - 10% PTFE - 2% Silicone  (discontinued **)
Data provided by PolyOne.
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber  (discontinued **)
Data provided by PolyOne.
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
PolyOne Lubri-Tech™ AT-15GP/05T Acetal With Graphite - 5% PTFE  (discontinued **)
Data provided by PolyOne.
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade
Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)...
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Ineos ABS Lustran® 720 ABS, Molding Grade
Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed..
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® 750 ABS, Molding Grade
Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl..
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® ABS 241 ABS, Blending Grade
Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade
Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan EX401 Copolyester
Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan LX150HF Copolyester
Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades ..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan LX201 Copolyester
Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan MX710 Copolyester
Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan MX711 Copolyester
Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan MX730 Copolyester
Eastman Tritan Copolyester MX730 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX730 is a high flow medical grade of Eastman Tritan that has viscosity re..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan MX731 Copolyester
Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan MX810 Copolyester
Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan MX811 Copolyester
Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceGood heat resistanceO..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan TX1000 Copolyester
Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan TX1001 Copolyester
Eastman Tritan TX1001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX1001 contains a mold release derived from vegetable based sources. Its most outstanding fe..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan TX1500HF Copolyester
Eastman Tritan TX1500HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1500HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1000. Other outstanding features..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan TX1501HF Copolyester
Eastman Tritan TX1501HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1501HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1001. Eastman Tritan copolyester..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan TX2000 Copolyester
Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc..
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Eastman Tritan TX2001 Copolyester