Processing Properties Metric English Comments
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Mold surface temperature at equilibrium conditions
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Mold surface temperature at equilibrium conditions
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Core surface temp. at equilibrium
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Core surface temp. at equilibrium
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Mold surface temperature at equilibrium conditions
NOVA Chemicals Dylark® 480P12 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Core surface temp. at equilibrium
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin
Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Core surface temp. at equilibrium
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Core surface temp. at equilibrium
NOVA Chemicals DYLARK® 250 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Mold surface temperature at equilibrium conditions
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Mold surface temperature at equilibrium conditions
NOVA Chemicals Dylark® 378P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Mold Temperature 43.0 - 60.0 °C
109 - 140 °F
Mold surface temperature at equilibrium conditions
NOVA Chemicals Dylark® 480P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Butyrate B9001-16H , 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 17% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 17% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 17% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 18% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade
Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)...
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® 750 ABS, Molding Grade
Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl..
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® ABS 241 ABS, Blending Grade
Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v..
Mold Temperature 43.0 - 66.0 °C
109 - 151 °F
Injection Molding
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade
Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v..
Mold Temperature 43.0 - 74.0 °C
109 - 165 °F
Average value: 56.0 °C Grade Count:21
Overview of materials for Cellulose Acetate Propionate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 35% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro..
Mold Temperature 43.0 °C
109 °F
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Copyright © lookpolymers.com All Rights Reserved