| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova FX550 (ASTM) Advanced Styrenic Polymer
(discontinued **)
Extremely high glossHigh Izod impact strengthUL Classification 94 HBPractical toughnessHigh flow for injection moldingScuff resistanceApplications: Replacement resin for selected ABS applicationsRef..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 1210 High Heat Crystal Polystyrene
(discontinued **)
High heat resistance, High molecular weight, optimum performance in extruded foamApplications: Meat and poultry trays, Egg cartons, Food packagingExposure to gamma radiation in the 2.02-6.06 megarad..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 1511 High Heat Crystal Polystyrene
(discontinued **)
High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 1531 High Heat Crystal Polystyrene
(discontinued **)
High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 2590 General Purpose Crystal Polystyrene
(discontinued **)
Good blending resin, Good balance of flow, strength and heat resistance, USP Class VIApplications: Consumer electronics, Housewares, Co-extrusion cap coat, Impact resin cuttingExposure to gamma radi..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 3700 General Purpose Crystal Polystyrene
(discontinued **)
Good balance of flow and strength, Good crack resistanceApplications: Single service wares, Blending resinExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the ..
|
|||
| Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
|
PolyOne Lubri-Tech™ AT-15GP/05T Acetal With Graphite - 5% PTFE
(discontinued **)
Data provided by PolyOne.
|
|||
| Mold Temperature | 38.0 - 79.0 °C | 100 - 174 °F | |
|
Samsung Cheil Industries Starex® HF-5330S ASA, Unreinforced
(discontinued **)
Amorphous Styrene Acrylonitrile (SAN)Characteristics: Heat Resistant: Impact and Chemical Resistance, Surface GlossApplications: Oil Filter Case, Lubricant Can, Refrigerator and Hair Dryer Component..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 1510 High Heat Crystal Polystyrene
High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 1600 High Heat Crystal Polystyrene
High heat resistance, Moderate flow, Good balance of strength and set-upApplications: Foam extrusion, Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant e..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 3101 General Purpose Crystal Polystyrene
Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 5410 High Impact Polystyrene
High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C ..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 6201 Super High Impact Polystyrene
Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined..
|
|||
| Mold Temperature | 38.0 - 93.0 °C | 100 - 199 °F | Injection Molding |
|
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade
Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g..
|
|||
| Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | Injection Molding |
|
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
|
|||
| Mold Temperature | 38.0 - 77.0 °C | 100 - 171 °F | |
|
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..
|
|||
| Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
|
Eastman Tritan LX150HF Copolyester
Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades ..
|
|||
| Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
|
Eastman Tritan TX1000 Copolyester
Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 1220 High Heat Crystal Polystyrene
(discontinued **)
Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 3511 General Purpose Crystal Polystyrene
(discontinued **)
Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 5104 High Impact Polystyrene
(discontinued **)
Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 5420 High Impact Polystyrene
(discontinued **)
High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 5500 High Impact Polystyrene
(discontinued **)
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio..
|
|||
| Mold Temperature | 38.0 °C | 100 °F | |
|
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 20% Plasticizer
(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
|
|||
| Mold Temperature | 38.0 - 93.3 °C | 100 - 200 °F | Average value: 69.8 °C Grade Count:22 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 2581 General Purpose Crystal Polystyrene
(discontinued **)
Good blending resin, Good balance of flow, strength and heat resistanceApplications: Consumer electronics, HousewaresExposure to gamma radiation in the 2.02-6.06 megarad range has no significant eff..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 5190 High Impact Polystyrene
(discontinued **)
Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C ..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 5530 High Impact Polystyrene
(discontinued **)
Good overall balance of properties, Good toughnessApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 6110 Super High Impact Polystyrene
(discontinued **)
Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen..
|
|||
| Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
|
Ineos Nova 1200 High Heat Crystal Polystyrene
Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia..
|
|||