Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Tritan MX811 Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Tritan
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Tritan MX811 Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceGood heat resistanceOutstanding impact resistanceQuick cycle timesProduct Description:Eastman Tritan MX811 is an amorphous copolyester with excellent appearance and clarity. Tritan MX811 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. This new generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Eastman Copolyester MX811 has been formulated for medical devices. Eastman Tritan Copolyester MX811 has been tested for FDA/ISO 10993 and USP Class VI Biological Evaluation testing after Gamma and ETO sterilization.Information provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 53.0 MPa
7690 psi
ASTM D638
Tensile Strength, Yield 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 140 %
140 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 1.585 GPa
229.9 ksi
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 1.585 GPa
229.9 ksi
ASTM D790
Izod Impact, Notched 6.50 J/cm
12.2 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C
228 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
ASTM D648
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Transmission, Visible 92 %
92 %
Total; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 260 - 282 °C
500 - 540 °F
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Drying Temperature 88.0 °C
190 °F
Dry Time 4 - 6 hour
4 - 6 hour