Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Tritan MX711 Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Tritan
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Tritan MX711 Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Copolyester MX711 has many outstanding features that include excellent toughness, hydrolytic stability, heat resistance, and chemical resistance. Eastman Tritan MX711 has been formulated for medical devices. Eastman Tritan copolyester MX711 has been tested for FDA/ISO 10993 and USP Class VI Biological Evaluation testing after Gamma and ETO sterilization.Application/UsesBlood therapyIV componentsKey AttributesEase of processingExcellent clarityExcellent hydrolytic stabilityFast cycle timesFast drying timesGood chemical resistanceGood color stability upon ETO sterilizationGood color stability upon gamma sterilizationGood heat resistanceOutstanding impact resistanceTypical properties as listed are from preliminary data. Information was provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength at Break 53.0 MPa
7690 psi
ASTM D638
Tensile Strength, Yield 43.0 MPa
6240 psi
ASTM D638
Elongation at Break 210 %
210 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 1.55 GPa
225 ksi
ASTM D638
Flexural Yield Strength 62.0 MPa
8990 psi
ASTM D790
Flexural Modulus 1.55 GPa
225 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Temperature -40.0 °C
2.06 ft-lb/in

@Temperature -40.0 °F
ASTM D256
9.80 J/cm

@Temperature 23.0 °C
18.4 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 61.0 J

@Temperature 23.0 °C
45.0 ft-lb

@Temperature 73.4 °F
Energy @ Max. Load; ASTM D3763
66.0 J

@Temperature -40.0 °C
48.7 ft-lb

@Temperature -40.0 °F
Energy @ Max. Load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature 260 - 282 °C
500 - 540 °F
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Drying Temperature 88.0 °C
190 °F
Dry Time 4 - 6 hour
4 - 6 hour