| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 238 - 249 °C | 460 - 480 °F | |
|
Nylene® 451 Nylon 6
Dry as molded. Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long produ..
|
|||
| Nozzle Temperature | 238 - 249 °C | 460 - 480 °F | |
|
Nylene® 451 Nylon 6, 50% RH
Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long product life to gears..
|
|||
| Nozzle Temperature | 238 °C | 460 °F | |
|
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced
Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor..
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
PTS Trimid® N6-200L Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
PTS Trimid® N6-200N Nylon 6 with Nucleating Agent
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6
Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
PTS Trimid® N6-G30L 30% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
PTS Trimid® N6-G33L 33% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin
(discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
DuPont Bexloy® AXW504BK Modified Ionomer Resin
(discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
DuPont Bexloy® AXW602NC010 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
(discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||
| Nozzle Temperature | 238 - 254 °C | 460 - 490 °F | |
|
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded
V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc.
|
|||
| Nozzle Temperature | 238 - 254 °C | 460 - 490 °F | |
|
LTL Color Compounds ColorFast® FRPBT210 PBT, Flame Retarded, Impact Modified
V-0 rated, impact modified unfilled PBTAll information provided by LTL Color Compounders, Inc.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
Diamond Polymers ABS/PC 7901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
Diamond Polymers ABS/PC 9901
Description: Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Diamond Polymers ABS/PC FC-30
Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Diamond Polymers ASA/PC FA-30
Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose
Data provided by Clariant Masterbatches
|
|||
| Nozzle Temperature | 238 - 266 °C | 460 - 510 °F | |
|
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
Diamond Polymers ABS/PC 8901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | Average value: 254 °C Grade Count:5 |
|
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
DuPont Bexloy® AXW502NC010 Modified Ionomer Resin
(discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||
| Nozzle Temperature | 238 - 254 °C | 460 - 490 °F | |
|
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded
Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
Diamond Polymers ABS/PC 9801
Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
(discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||