| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
| Melt Flow | 1.0 g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C |
1.0 g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
| 4.9 g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C |
4.9 g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 111 | 111 | ASTM D785 |
| Tensile Strength, Yield | 42.1 MPa | 6100 psi | chs 2 in/min; ASTM D638 |
| Flexural Modulus | 1.79 GPa | 260 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
| Izod Impact, Notched | 5.07 J/cm <br>@Thickness 3.17 mm,<br> Temperature 23.0 °C |
9.50 ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F |
bar; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
| 103 °C | 217 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 | |
| Vicat Softening Point | 122 °C | 251 °F | 0.125 inch, 1 Kg; ASTM D1525 |
| Flammability, UL94 | HB <br>@Thickness 1.50 mm |
HB <br>@Thickness 0.0591 in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
| Middle Barrel Temperature | 235 - 266 °C | 455 - 510 °F | |
| Front Barrel Temperature | 238 - 271 °C | 460 - 520 °F | |
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
| Melt Temperature | 238 - 271 °C | 460 - 520 °F | Melt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability. |
| Mold Temperature | 37.8 - 82.2 °C | 100 - 180 °F | Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products. |
| Drying Temperature | 90.6 - 98.9 °C | 195 - 210 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
| Moisture Content | <= 0.020 % | <= 0.020 % | |
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi |