| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.020 | 0.020 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm <br>@Thickness 3.20 mm |
0.0040 - 0.0060 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 5.0 g/10 min <br>@Load 2.16 kg,<br> Temperature 250 °C |
5.0 g/10 min <br>@Load 4.76 lb,<br> Temperature 482 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 111 | 111 | ASTM D785 |
| Tensile Strength, Yield | 54.9 MPa <br>@Thickness 3.20 mm |
7970 psi <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | 100 % <br>@Thickness 3.20 mm |
100 % <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Flexural Yield Strength | 88.3 MPa <br>@Thickness 3.20 mm |
12800 psi <br>@Thickness 0.126 in |
10mm/min; ASTM D790 |
| Flexural Modulus | 2.26 GPa <br>@Thickness 3.20 mm |
327 ksi <br>@Thickness 0.126 in |
10mm/min; ASTM D790 |
| Izod Impact, Notched | >= 4.90 J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C |
>= 9.18 ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F |
ASTM D256 |
| >= 5.88 J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C |
>= 11.0 ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 112 °C <br>@Thickness 6.40 mm |
234 °F <br>@Thickness 0.252 in |
Unannealed; ASTM D648 |
| UL RTI, Electrical | 60.0 °C <br>@Thickness >=0.750 mm |
140 °F <br>@Thickness >=0.0295 in |
|
| UL RTI, Mechanical with Impact | 60.0 °C <br>@Thickness >=0.750 mm |
140 °F <br>@Thickness >=0.0295 in |
|
| UL RTI, Mechanical without Impact | 60.0 °C <br>@Thickness >=0.750 mm |
140 °F <br>@Thickness >=0.0295 in |
|
| Flammability, UL94 | HB <br>@Thickness >=0.750 mm |
HB <br>@Thickness >=0.0295 in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
| Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
| Front Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
| Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
| Melt Temperature | 255 - 285 °C | 491 - 545 °F | Injection Molding |
| Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
| Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
| Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour | Injection Molding |
| Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |