Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 254 - 277 °C | 489 - 531 °F | |
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Front Barrel Temperature | 254 - 277 °C | 489 - 531 °F | |
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Front Barrel Temperature | 243 - 277 °C | 470 - 530 °F | |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Front Barrel Temperature | 243 - 277 °C | 470 - 530 °F | |
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 243 - 277 °C | 470 - 530 °F | |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Front Barrel Temperature | 238 - 277 °C | 460 - 530 °F | |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Front Barrel Temperature | 238 - 277 °C | 460 - 530 °F | |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Front Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Front Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
Ravago Manufacturing Americas Hybrid B6720U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Front Barrel Temperature | 243 - 277 °C | 470 - 530 °F | |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Front Barrel Temperature | 243 - 277 °C | 470 - 530 °F | |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Front Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Front Barrel Temperature | 249 - 277 °C | 480 - 530 °F | |
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Firestone CG430-203 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Front Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
LTL Color Compounds ColorFast® FRPBT130 PBT, 30% Glass-Filled 30% glass-filled V-0 rated PBT - UL listedAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 271 - 277 °C | 520 - 530 °F | |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6 Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman. |
|||
Front Barrel Temperature | 260 - 277 °C | 500 - 530 °F | |
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Front Barrel Temperature | 260 - 277 °C | 500 - 530 °F | |
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Front Barrel Temperature | 260 - 277 °C | 500 - 530 °F | |
Wellman Wellamid® GS40-66 22L-N 40% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Front Barrel Temperature | 260 - 277 °C | 500 - 530 °F | |
Wellman Wellamid® GSF25/15-66 22L-N 40% Glass Sphere/Fiber Reinforced Nylon 66 Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 265 - 277 °C | 509 - 531 °F | |
Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer go.. |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Elastocon TPE Technologies Elastocon® STK56PA-B Thermoplastic Elastomer Elastocon® STK56PA-B black thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA-B is well suited for .. |
|||
Front Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Front Barrel Temperature | 238 - 277 °C | 460 - 530 °F | |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 238 - 277 °C | 460 - 530 °F | |
Polymer Resources PPX-FR2 Modified PPO, UL 94 V-1 with HDT of 210 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 238 - 277 °C | 460 - 530 °F | |
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |