Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
PolyOne Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Front Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G20 Nylon 6, 20% Glass Reinforced Nylon 6, 20% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G33 Nylon 6, 33% Glass Reinforced Nylon 6, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Front Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FRG7.5 Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 511 °F | |
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th.. |
|||
Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-M25G15 Nylon 6, 25% Mineral, 15% Glass Reinforced Nylon 6, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gra.. |
|||
Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Front Barrel Temperature | 249 °C | 480 °F | |
MTI ThermoStran® PP-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Front Barrel Temperature | 249 °C | 480 °F | |
MTI ThermoStran® TPU-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Front Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions. |