Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 266 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Front Barrel Temperature 266 - 304 °C
510 - 580 °F
Polymer Resources PPX-GP3 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Front Barrel Temperature 266 - 304 °C
510 - 580 °F
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow
Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Front Barrel Temperature 266 - 304 °C
510 - 580 °F
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant
Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan..
Front Barrel Temperature 266 - 304 °C
510 - 580 °F
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 266 - 277 °C
510 - 530 °F
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled
Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone
Front Barrel Temperature 266 - 293 °C
510 - 560 °F
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled
13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 266 - 293 °C
510 - 560 °F
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified
13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 266 - 293 °C
510 - 560 °F
LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled
33% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 266 - 277 °C
510 - 530 °F
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6
Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman.
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® 22LHI6 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® 22LH-N Unfilled Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Front Barrel Temperature 266 - 277 °C
510 - 530 °F
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Front Barrel Temperature 266 - 277 °C
510 - 530 °F
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® T-731E-BK 10% Reinforced Abrasion Resistant Nylon 6
Description: Abrasion Resistant Nylon 6Information provided by Wellman.
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® XT1482-BK High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Front Barrel Temperature 266 - 282 °C
510 - 540 °F
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66
Description: Medium Impact Nylon 66Information provided by Wellman.
Front Barrel Temperature 266 - 271 °C
510 - 520 °F
Diamond Polymers ASA M-523
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Front Barrel Temperature 266 - 293 °C
510 - 560 °F
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized
Data provided by Clariant Masterbatches
Front Barrel Temperature 266 - 293 °C
510 - 560 °F
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
Front Barrel Temperature 266 - 277 °C
510 - 530 °F
Elastocon TPE Technologies Elastocon® STK56PA-B Thermoplastic Elastomer
Elastocon® STK56PA-B black thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA-B is well suited for ..
Front Barrel Temperature 266 - 304 °C
510 - 580 °F
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 266 - 293 °C
510 - 560 °F
LTL Color Compounds ColorFast® NY1 Nylon 6
Injection molding nylon 6, with or without lubeAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 266 - 293 °C
510 - 560 °F
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled
13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 266 - 293 °C
510 - 560 °F
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled
33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc.
Copyright © lookpolymers.com All Rights Reserved