Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by.. |
|||
Front Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
Polymer Resources PCSF-FR G30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond.. |
|||
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
Polymer Resources PCSF-FRG30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Polycarbonate, 30% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Front Barrel Temperature | 260 - 310 °C | 500 - 590 °F | |
Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer Impact modified, UV stabilizedThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where low.. |
|||
Front Barrel Temperature | 260 - 310 °C | 500 - 590 °F | |
Hybrid Plastics CO6U50.02 Nanoreinforced® Cyclic Olefin Copolymer Impact modified, flame retardantThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where l.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | Injection Molding |
LG Chemical LUCON PO6062 mPPO+CNT+CF+GF Description: Injection Molding, mPPO+CNT+CF+GF, High Strength, Heat StabilityApplication: ATM parts, LCD Cell TrayCAS No. 35134-01-4, 25038-54-4, 65997-17-3, 7440-44-0 and 7782-42-5Information provi.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | Injection Molding |
LG Chemical LUCON PO6063 mPPO+CNT+CF+GF Description: Injection Molding, mPPO+CNT+CF+GF, Electrostatic Dissipation, High Strength, Low WarpageApplication: LCD Cell TrayCAS No. 35134-01-4, 65997-17-3, 7440-44-0 and 7782-42-5Information prov.. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUPOY SC1004A PC Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |
|||
Front Barrel Temperature | 293 - 310 °C | 560 - 590 °F | |
Polymer Resources PCSF-FR1 Polycarbonate, 10% Glass Reinforced Structural Foam Grade Polycarbonate, 10% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-FRG10 Modified PPO, UL 94 V-1, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUCON CP6067 PC+CNT+CF Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74.. |