Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 240 °C | 464 °F | |
Multibase TPSiV™ 1180-50D Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Middle Barrel Temperature | 240 - 255 °C | 464 - 491 °F | |
Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer
(discontinued **) Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt .. |
|||
Middle Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Start Point: 250°C |
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 235°C |
Kingfa MAC-601 UV PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 235°C |
Kingfa PC-S609 Toughened PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Middle Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
LG Chemical LUMID GP2130AE PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Industrial MaterialCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® HI2152 PBT+GF15% Description: Injection Molding, PBT+GF15%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® LW5300M PBT+PC+MF30% Description: Injection Molding, PBT+PC+MF30%, Low WarpageApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 103598-77-2, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® LW5402A PBT+PC+GF40% Description: Injection Molding, PBT+PC+GF40%, Low Warpage, High GlossApplication: E&E, Automotive (Bobbin, Switch)CAS No. 9010-86-0, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® SG3180S PBT+PET+MF18% Description: Injection Molding, PBT+PET+MF18%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 255 °C | 464 - 491 °F | Injection Molding |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Middle Barrel Temperature | 240 - 255 °C | 464 - 491 °F | Injection Molding |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Middle Barrel Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY GP-5000FQ General Purpose PC/ABS Alloy, Unreinforced, Excellent Flow Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Middle Barrel Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced Vyteen PC/ABS 3016 is a black 16% glass fiber reinforced Polycarbonate/ABS alloy designed for injection molding.Features: -Good processability -Balanced stiffness/resilience -High deflection temp.. |
|||
Middle Barrel Temperature | 240 - 255 °C | 464 - 491 °F | Injection Molding |
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 255 °C | 464 - 491 °F | |
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Teknor Apex Beetle® MD82 Nylon 6, Non-halogenated, Dry Notes: MD82 is a UL recognized, V-0 rated halogen and phosphorus-free flame retarded, heat stabilized, unreinforced injection molding grade of nylon 6; U.L. 94 V-O at 0.63mm. Colorable Features: Fla.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Teknor Apex Beetle® MDM54 Nylon 6, Non-halogenated, Mineral Reinforced Notes: MDM54 is a UL recognized, V-2 rated halogen and phosphorus-free flam retarded, mineral filled injection molding grade of nylon 6, primarily intended for electrical applications; U.L. 94 V-2 a.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Unitika AX-1500 Conditioned AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Unitika UM-8430RG Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Zone 2 |
Eurostar Staramide PF004EUC PA6, 20% Glass Filled, Injection Molded PF004EUC is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Zone 2 |
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 240 - 280 °C | 464 - 536 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) ST6010 Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |