Processing Properties Metric English Comments
Injection Pressure 4.83 - 150 MPa
700 - 21800 psi
Average value: 73.3 MPa Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Injection Pressure 4.83 - 103 MPa
700 - 15000 psi
Average value: 53.6 MPa Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 1000
Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 1501E
Description: Extrusion GradeInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3002MC
Description: Plating GradeInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3003 MC
Description: High Heat Plating GradeInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3003MC Black 1722
Description: BlackInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3500 Natural 1050
Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3501 GF-30
Description: Reinforced Grade, 30%Glass FilledInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3501 Natural 1000 P
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3502
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3502E
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 6.21 MPa
700 - 900 psi
Diamond Polymers ABS 3502ELG
Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 4000HH
Description: Heat Resistant Grade, Medium High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 6.21 MPa
700 - 900 psi
Diamond Polymers ABS 4000HH-ELG
Description: Heat Resistant Grade, Low Gloss, Medium High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 4001H3F
Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 4003HH
Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 4011 HH
Description: Ultra High Heat ABSInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 4500R
Description: Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 6.21 MPa
700 - 900 psi
Diamond Polymers ABS 7600B (ELG)
Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 9502
Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 9502E
Description: Extrusion Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS TM 25
Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS TM 35
Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS TM 40
Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS TX-541
Description: Super High Heat ABSInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers TR 5000
Description: Transparent ABSInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 150 MPa
700 - 21800 psi
Average value: 61.7 MPa Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 1100
Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3500B
Description: Blow Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.