| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded | 
| Manufacturer | Diamond and Network Polymers | 
| Trade Name | |
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Diamond Polymers ABS 1501E.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 | 
| Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 | 
| Melt Flow | 0.50           g/10 min @Load 5.00 kg, Temperature 200 °C | 0.50           g/10 min @Load 11.0 lb, Temperature 392 °F | Procedure A Condition G; ASTM D1238 | 
| 1.8           g/10 min @Load 3.80 kg, Temperature 230 °C | 1.8           g/10 min @Load 8.38 lb, Temperature 446 °F | Procedure A Condition I; ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell R | 112 | 112 | ASTM D785 | 
| Tensile Strength, Yield | 49.0 MPa | 7100 psi | chs 2 in/min; ASTM D638 | 
| Flexural Modulus | 2.43 GPa | 353 ksi | Tangent, chs 0.05 in/min; ASTM D790 | 
| Izod Impact, Notched | 1.33           J/cm @Thickness 3.17 mm, Temperature 23.0 °C | 2.50           ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F | bar; ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 | 
| 95.0 °C | 203 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 | |
| Vicat Softening Point | 104 °C | 219 °F | 0.125 inch, 1 Kg; ASTM D1525 | 
| Flammability, UL94 | HB @Thickness 1.50 mm | HB @Thickness 0.0591 in | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Middle Barrel Temperature | 190 - 250 °C | 374 - 482 °F | |
| Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | Higher mold temperature provides a product with excellent surface finishing and less residual stress. | 
| Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
| Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi |