Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
7.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 101 | 101 | ASTM D785 |
Tensile Strength, Yield | 43.4 MPa | 6300 psi | chs 2 in/min; ASTM D638 |
Flexural Modulus | 2.28 GPa | 330 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Izod Impact, Notched | 3.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
6.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
93.3 °C | 200 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 | |
Vicat Softening Point | 103 °C | 218 °F | 0.125 inch, 1 Kg; ASTM D1525 |
UL RTI, Electrical | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | |
Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | Higher mold temperature provides a product with excellent surface finishing and less residual stress. |
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi |