Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 44.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 50.0 - 80.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
27.8 - 44.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Nylacast Impact Nylon 6, Impact Grade
Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also..
CTE, linear 60.0 - 80.0 µm/m-°C
33.3 - 44.4 µin/in-°F
Polykemi
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
CTE, linear 60.0 - 80.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
33.3 - 44.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Cycoloy® MC8200 PC+ABS (Asia Pacific)
CTE, linear 60.0 - 80.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
33.3 - 44.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Lexan® LCR200 PBT+PC (Asia Pacific)
CTE, linear 60.0 - 80.0 µm/m-°C
33.3 - 44.4 µin/in-°F
Polykemi
Polykemi AB POLYfill PP EIP8020F Polypropylene/EPDM, Mineral Reinforced
Information provided by Polykemi AB
CTE, linear 71.0 - 80.0 µm/m-°C
39.4 - 44.4 µin/in-°F
Average value: 72.5 µm/m-°C Grade Count:6
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
CTE, linear 60.0 - 80.0 µm/m-°C
33.3 - 44.4 µin/in-°F
Polykemi
Polykemi AB POLYfill PPH T16020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
CTE, linear 60.0 - 80.0 µm/m-°C
33.3 - 44.4 µin/in-°F
Average value: 71.7 µm/m-°C Grade Count:3
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
CTE, linear 63.0 - 80.0 µm/m-°C
35.0 - 44.4 µin/in-°F
Average value: 68.7 µm/m-°C Grade Count:3
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
CTE, linear 24.0 - 80.0 µm/m-°C
13.3 - 44.4 µin/in-°F
Average value: 52.7 µm/m-°C Grade Count:3
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
CTE, linear 18.0 - 80.0 µm/m-°C
10.0 - 44.4 µin/in-°F
Average value: 27.3 µm/m-°C Grade Count:19
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
CTE, linear 1.50 - 80.0 µm/m-°C
0.833 - 44.4 µin/in-°F
Average value: 23.9 µm/m-°C Grade Count:23
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
CTE, linear 20.0 - 80.0 µm/m-°C
11.1 - 44.4 µin/in-°F
Average value: 43.3 µm/m-°C Grade Count:21
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Conditioned
Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Conditioned
Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned
Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Dry
Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned
Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Dry
Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Dry
Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 70.0 - 80.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 - 44.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL GTX GTX6009 PPE+PS+PA6 (Asia Pacific)
PA6 based unfilled GTX for Wheel cover
CTE, linear 70.0 - 80.0 µm/m-°C
38.9 - 44.4 µin/in-°F
Hippe PET Polyethylene Terephthalate
Linear, saturated polyesters are thermoplastics which are used where good dimensional accuracy, high creep resistance and good sliding and wear behavior are required. Partially crystallized PET pos..
CTE, linear 60.0 - 80.0 µm/m-°C

@Temperature 20.0 °C
33.3 - 44.4 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance BIN-45 Bonded (Composite) Magnetic Material
CTE, linear 10.0 - 80.0 µm/m-°C
5.56 - 44.4 µin/in-°F
Average value: 57.5 µm/m-°C Grade Count:7
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
CTE, linear 70.0 - 80.0 µm/m-°C
38.9 - 44.4 µin/in-°F
Hippe PVC-U Polyvinyl Chloride
Material at reasonable price, high strength. Used in machine construction as covers, pipes, section, façade elements.Information provided by Hippe.
CTE, linear 50.0 - 80.0 µm/m-°C
27.8 - 44.4 µin/in-°F
Average value: 55.4 µm/m-°C Grade Count:5
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
CTE, linear 3.30 - 80.0 µm/m-°C
1.83 - 44.4 µin/in-°F
Average value: 31.4 µm/m-°C Grade Count:59
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..
Copyright © lookpolymers.com All Rights Reserved