Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
DSM Arnite® TV4 460 KL TV4 460 PBT/PET Blend-30% Glass Reinforced (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
Nilit FRIANYL B63 GV10 Nylon 6 for injection molding, 10% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
Nilit FRIANYL B63 HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
Nilit FRIANYL C73 MG40 Nylon 6.6/6 for injection molding, 40% mineral filled Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN333HI2 High Impact Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ASTM D648 |
Kolon SPESIN® KP213G30SB3 Glass Fiber Reinforced PBT Compound Resin G/F 30% reinforcedApplications: Ignition coil bobbinsInformation provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
Lanxess Pocan® KL 1-7033 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, impact modified |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East) Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 20 HWCP 20% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/2 |
Eurotec® Tecodur® PB70 GR15 NL PBT 15% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/2 |
Eurotec® Tecomid® NB40 GR25 NL PA 6 25% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
Barlog Plastics KEBATER BF120 PBT, 20% glass fiber reinforced PBT-GF20Information provided by BARLOG plastics GmbH. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
BASF Ultradur B 4300 G3 15% Glass Filled PBT Ultradur B 4300 G3 is an easy flowing injection molding PBT with 15% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
BASF Ultramid® TG7S BK-102 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified nylon 6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
BASF Ultradur B 4406 G6 Q717 30% Glass Filled PBT Ultradur B 4406 G6 Q717 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
DSM Arnite® TV6 241 SN PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C @Thickness 3.20 mm |
428 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP 9X11427 LNP* THERMOCOMP* 9X11427 is a compound based on Miscellanbeous resin containing 40% specialty glass filled TP alloy. Added features of this grade include: Ultra-Stiff Toughness, Improved Impact, G.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East) VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-2 |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | DIN 53461 |
Polyram RamSter PF303G4 PBT, 20% Glass Fiber 20% Glass-fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
Lanxess Pocan® B 3235 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, improved flowability |