Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 263 °C | 505 °F | ASTM D789 |
NYCOA 5033 HS 33% Glass-Fiber Reinforced, Heat Stabilized, Nylon 66 Resin NYCOA 5033 HS is a 33% glass fiber reinforced, heat stabilized Nylon 66 resin used for injection molding. It offers an outstanding balance of mechanical properties over standard grades of convention.. |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66
(Unverified Data**) Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po.. |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66
(Unverified Data**) Zytel® ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance, high productivity and laser markability.Information provided by DuPont |
|||
Melting Point | 263 °C | 505 °F | DAM |
Aardvark Polymers Aarlon® 4055FR PA 6/6 Rotational Molding Resin Aarlon 4055FR is a premium flame retardant type 6/6 nylon.Aarlon 4055FR is halogen, heavy metal, and red phosphorus free.Aarlon 4055FR is UL94 V-0 rated.Aarlon 4055FR is semi-crystalline, nucleated,.. |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 221 Natural FA PA66, DRY Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 225F PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, Conditioned Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This p.. |
|||
Melting Point | 263 °C | 505 °F | ASTM D3418 |
Samyang Tramid® 210G35 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G35 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, DRY Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Melting Point | 263 °C | 505 °F | ISO 3146-C |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66 Unreinforced High Viscosity Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FG50 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66
(Unverified Data**) Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | ASTM D789 |
Adell AR-37 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 263 °C | 505 °F | ASTM D789 |
Adell AR-17 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 263 °C | 505 °F | DAM; ASTM D3418 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Zytel® FG408L NC010 is a general purpose, lubricated, impact modified polyamide 66 resin with superior toughness for injection molding applications. It has been developed for consideration into app.. |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**) Zytel® FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont Performance.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T.. |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS BK099 is a 14% glass fiber reinforced toughened high flow heat stabilized black polyamide 66 resin. It offers outstanding p.. |