Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
33% Glass Reinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
DAM; ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
DAM; ISO 527-1/-2
Tensile Modulus 10.5 GPa
1520 ksi
DAM; ISO 527-1/-2
Flexural Strength 290 MPa
42100 psi
DAM; ISO 178
Flexural Modulus 9.30 GPa
1350 ksi
DAM; ISO 178
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
DAM; ISO 75-1/-2
Descriptive Properties Value Comments
Part Marking Code >PA66-GF33<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA66-GF33