Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Asia Pacific) |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
LNP ULTEM® JD7902 Polyetherimide
(discontinued **) Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.. |
|||
Flexural Modulus | 5.88 GPa @Thickness 3.20 mm |
853 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID LW4303B(W) PA66+MF30%, Low Warpage Feature: Injection Molding, PA66+MF30%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D570 |
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN132G15VO G/F Reinforced Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
LG Chemical LUPOL LW-4407 Low Warpage Polypropylene, 40% Glass Fiber/Mineral Filler Reinforced, Heat Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Modulus | 5.88 GPa @Thickness 3.20 mm |
853 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 5.88 GPa @Thickness 3.20 mm |
853 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D 790 |
SABIC Innovative Plastics Ultem JD7902 PEI (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific) 20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HT-8200G MPPE/PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VG-4920 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HT-8200G MPPE/PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
PlastxWorld CEVIAN® SERG2 20% GF ABS Glass fiber reinforced and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
PlastxWorld CEVIAN® SKG20 20% GF ABS Glass fiber reinforced, heat resistant and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plast.. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 30G3F Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60G3F Nylon 66, 15% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) ST60G6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D 790 |
SABIC Innovative Plastics Valox® VGF4715 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubric.. |