Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN® SKG20 20% GF ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® SKG20 20% GF ABS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Glass fiber reinforced, heat resistant and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 83.4 MPa
12100 psi
ASTM 638
Flexural Yield Strength 118 MPa
17100 psi
ASTM D790
Flexural Modulus 5.88 GPa
853 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
0.5 inch unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in