| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Cycoloy® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Water Absorption | 0.20 % <br>@Time 86400 sec |
0.20 % <br>@Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm <br>@Thickness 3.20 mm |
0.0020 - 0.0040 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 107 MPa | 15500 psi | SABIC - Japan Method |
| Elongation at Break | 7.0 % | 7.0 % | SABIC - Japan Method |
| Flexural Strength | 113 MPa | 16400 psi | ASTM D790 |
| Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
| Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 30.0 - 50.0 µm/m-°C <br>@Temperature -30.0 - 30.0 °C |
16.7 - 27.8 µin/in-°F <br>@Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 0.46 MPa (66 psi) | 100 °C <br>@Thickness 3.20 mm |
212 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Flammability, UL94 | V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
UL 94 |
| 5VA <br>@Thickness 2.50 mm |
5VA <br>@Thickness 0.0984 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |