| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP THERMOCOMP |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.352 g/cc | 0.04884 lb/in³ | ASTM D792 |
| Water Absorption | 0.17 % @Time 86400 sec |
0.17 % @Time 24.0 hour |
ISO 62-1 |
| Moisture Absorption | 0.130 % | 0.130 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.0080 cm/cm @Time 86400 sec |
0.0060 - 0.0080 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 102 MPa | 14800 psi | Type I, 5 mm/min; ASTM D638 |
| 103 MPa | 14900 psi | 5 mm/min; ISO 527 | |
| Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
| 105 MPa | 15200 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 3.2 % | 3.2 % | Type I, 5 mm/min; ASTM D638 |
| 3.3 % | 3.3 % | 5 mm/min; ISO 527 | |
| 3.7 % | 3.7 % | Flexural Strain, break, 2 mm/min; ISO 178 | |
| Elongation at Yield | 2.9 % | 2.9 % | Type I, 5 mm/min; ASTM D638 |
| 3.0 % | 3.0 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 5.72 GPa | 830 ksi | 1 mm/min; ISO 527 |
| 6.10 GPa | 885 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 163 MPa | 23600 psi | 2 mm/min; ISO 178 |
| 169 MPa | 24500 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Yield Strength | 163 MPa | 23600 psi | 2 mm/min; ISO 178 |
| 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 5.88 GPa | 853 ksi | 2 mm/min; ISO 178 |
| 6.07 GPa | 880 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | Light & White Colors; ASTM D256 |
| 1.25 J/cm | 2.34 ft-lb/in | Natural & Black Colors; ASTM D256 | |
| Izod Impact, Unnotched | 8.95 J/cm | 16.8 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 53.0 kJ/m² | 25.2 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 28.9 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| CTE, linear, Transverse to Flow | 53.9 µm/m-°C @Temperature -30.0 - 30.0 °C |
29.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 141 °C @Thickness 3.20 mm |
286 °F @Thickness 0.126 in |
unannealed; ASTM D648 |