Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY CR3020 ASA Low-gloss ASA for profile and capstock applications |
|||
Dart Drop, Total Energy | 4.00 - 55.0 J | 2.95 - 40.6 ft-lb | Average value: 12.6 J Grade Count:7 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer (Asia Pacific) LNP* Lubricomp* KCL34A is a compound based on Acetal Homopolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear .. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240A PP SABIC® PPcompound G3240A is a general purpose, 40% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 139448304. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 4012G PBT VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | ASTM D3763 |
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66 LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66 LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WF0039U PBT LNP* THERMOCOMP* WF0039U is a compound based on PBT resin containing 15% Glass Fiber. Added features of this grade include: Flame Retardant and UV Stabilized. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific) LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450EX PBT (Asia Pacific) LNP* Thermocomp* WH0450EX is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP MX89510 PP LNP* THERMOCOMP* MX89510 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT (Asia Pacific) LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East) A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |