| Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP LUBRICOMP |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
| 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 | |
| Moisture Absorption | 0.100 % | 0.100 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0197 - 0.025 cm/cm <br>@Time 86400 sec |
0.0197 - 0.025 in/in <br>@Time 24.0 hour |
ASTM D955 |
| 0.0197 - 0.025 cm/cm <br>@Time 86400 sec |
0.0197 - 0.025 in/in <br>@Time 24.0 hour |
ISO 294 | |
| Linear Mold Shrinkage, Transverse | 0.0197 - 0.025 cm/cm <br>@Time 86400 sec |
0.0197 - 0.025 in/in <br>@Time 24.0 hour |
ASTM D955 |
| 0.0197 - 0.025 cm/cm <br>@Time 86400 sec |
0.0197 - 0.025 in/in <br>@Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 46.0 MPa | 6670 psi | ASTM D638 |
| 47.0 MPa | 6820 psi | ISO 527 | |
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
| 48.0 MPa | 6960 psi | ISO 527 | |
| Elongation at Break | 20.3 % | 20.3 % | ISO 527 |
| 22.3 % | 22.3 % | ASTM D638 | |
| Elongation at Yield | 10.8 % | 10.8 % | ISO 527 |
| 11.3 % | 11.3 % | ASTM D638 | |
| Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
| 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 59.0 MPa | 8560 psi | ISO 178 |
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
| 2.10 GPa | 305 ksi | ISO 178 | |
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 6.72 J/cm | 12.6 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
| Coefficient of Friction, Dynamic | 0.24 | 0.24 | ASTM D3702 Modified |
| Coefficient of Friction, Static | 0.13 | 0.13 | ASTM D3702 Modified |
| K (wear) Factor | 20.1 x 10<sup>-8</sup> mm³/N-M | 10.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 117 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 117 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
65.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 115 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
63.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 115 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
63.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 146 °C | 295 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 153 °C <br>@Thickness 3.20 mm |
307 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 83.0 °C | 181 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 84.0 °C <br>@Thickness 3.20 mm |
183 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |