| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Dart Drop, Total Energy | 4.00 - 55.0 J | 2.95 - 40.6 ft-lb | Average value: 12.6 J Grade Count:7 |
|
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12
LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated.
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12
LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer (Asia Pacific)
LNP* Lubricomp* KCL34A is a compound based on Acetal Homopolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear ..
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS
LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant.
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP
SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QCL349 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, Flame Retardant, Elect..
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
|
SABIC Innovative Plastics SABIC PPCOMPOUND G3240A PP
SABIC® PPcompound G3240A is a general purpose, 40% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 139448304.
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP RL4040HSUV PA 66
LNP* LUBRICOMP* RL4040HSUV is a compound based on Nylon 66 containing 20% PTFE. Added features of this grade include: Heat Stabilized, UV Stabilized, Wear Resistant.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA
LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA
LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific)
LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP STAT-KON KX96321 POM
LNP* STAT-KON* KX96321 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific)
LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP KB003RXZ Acetal Copolymer
LNP THERMOCOMP* KB003RXZ is a compound based on Acetal Copolymer resin containing 15% Glass Bead. Added features of this material include: Easy Release.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific)
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66
LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66
LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare.
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT
LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber.
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP WF0039U PBT
LNP* THERMOCOMP* WF0039U is a compound based on PBT resin containing 15% Glass Fiber. Added features of this grade include: Flame Retardant and UV Stabilized.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
|
|||
| Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0450EX PBT (Asia Pacific)
LNP* Thermocomp* WH0450EX is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP
LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP MX89510 PP
LNP* THERMOCOMP* MX89510 is a compound based on Polypropylene resin containing Proprietary Filler(s).
|
|||
| Dart Drop, Total Energy |
4.00
J <br>@Temperature 23.0 °C
|
2.95
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
|
|||
| Dart Drop, Total Energy | 4.00 - 19.0 J | 2.95 - 14.0 ft-lb | Average value: 11.8 J Grade Count:26 |
|
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||